試驗材料
|
試驗方式
|
試驗條件
|
適用規范
|
規范要求
|
化銀層
|
高溫高濕試驗
|
40℃/90%/196h
|
|
|
高Tg耐熱電路板
|
沖擊試驗
|
-65℃←→150℃/30min/1000cycle
|
|
|
電路板
|
沖擊試驗
|
-55℃←→125℃/30min/1000cycle
|
|
|
電路板
|
HAST試驗
|
135℃/85%/5.5V/500h
|
|
|
電路板
|
PCT吸濕率試驗
|
121℃/100%/5h
|
|
|
貫孔用導電銅膏
|
高溫高濕試驗
|
40℃/90%/1000h
|
|
|
貫孔用導電銅膏
|
高溫高濕試驗
|
60℃/95%/1000h
|
|
|
貫孔用導電銅膏
|
沖擊試驗
|
-55℃←→125℃/30min/200cycle
|
|
|
貫孔用導電銅膏
|
沖擊試驗
|
-55℃(9min)←室溫1min→125℃(9min)/1000cycle
|
|
|
貫孔用導電銅膏
|
PCT吸濕率試驗
|
121℃/100%/8h
|
|
|
FPC導電性接著膜
|
耐濕性
|
60℃/95%/1000h(電阻變化率50%以下)
|
|
電阻變化率50%以下
|
FPC電磁波屏蔽膜
|
彎曲試驗
|
溫度23℃/距離/30cm/(次數1000次/分鐘)
|
|
|
FPC電鍍材料
|
沖擊+MLR試驗
|
-55℃(5min)←→125℃(5min)/1000cycle/轉換時間10sec
|
MIL-P-5510
J-STD-003
|
|
PWB鍍銅材料
|
液體沖擊試驗
|
-55℃(5min)←→125℃(5min)/500cycle/轉換時間4sec
|
|
電阻變化率50%以下
|
PWB鍍銅材料
|
沖擊試驗
|
-65℃(5min)←→125℃(5min)/1000cycle/轉換時間10sec
|
|
電阻變化率50%以下
|
FPC
|
彎曲試驗
|
|
JIS C 6471
|
|
FPC
|
PCT吸濕率試驗
|
121℃/100%/192h
|
|
|
FPC
|
HAST試驗
|
120℃/85%/100V/100h/(50/50um)
|
|
|
FPC
|
彎曲試驗
|
溫度25℃/R=2mm/距離12cm/速度100rpm/次數180千次)
|
IPC-650-2.6.4.3
(未貼保護膠)
|
電阻變化率10%以下
|
FPC
|
高速高溫彎曲試驗
|
溫度75℃/R=2mm/距離12cm/速度1000rpm/次數2400千次)
|
IPC-650-2.6.4.3
(未貼保護膠)
|
電阻變化率10%以下
|